The Wintact WT100A listing describes one-sided ultrasonic thickness measurement from 1.00 to 225.0 mm using a 5 MHz probe. For a corroded plate, the hard part is rarely collecting one number. It is choosing locations ...

By EkoDeluxe · Published · Updated

Wintact WT100A product view

The Wintact WT100A listing describes one-sided ultrasonic thickness measurement from 1.00 to 225.0 mm using a 5 MHz probe. For a corroded plate, the hard part is rarely collecting one number. It is choosing locations so that a low spot does not disappear inside a convenient average.

Wintact WT100A product view

Wintact WT100A — supplier product view.

Wintact WT100A second product view

A second supplier view used to confirm the exact model and interface.

Think in a survey grid

A recent engineering discussion about aircraft damage describes mapped areas being ultrasonic thickness tested, while an X search result warns that corrosion does not distribute itself evenly and can pit. Those phrases support a grid mindset, not a promise of aviation-grade inspection. Mark rows and columns around the suspect area, including sound-looking metal outside it. Give every point a coordinate.

Workflow diagram for Wintact WT100A

Original workflow diagram: the record keeps setup, observation and boundary together.

Make the contact routine consistent

Clean loose scale, apply the instructed couplant and keep probe pressure and angle as consistent as the surface allows. The WT100A source supports the probe and range; it does not establish a universal couplant, calibration block or acceptance threshold. Record the material, surface condition, probe and any point that produced an unstable echo.

Keep the minimum visible

For each location write the first stable value, the minimum repeat value and a short confidence note. Photograph the marked grid and keep the data beside the drawing. Do not replace a cluster of low points with a single mean. A local minimum may be the decision that sends a part for a qualified inspection.

Separate screening from certification

The resulting map can help prioritise maintenance and identify where more qualified NDT is needed. It cannot by itself certify remaining life, weld integrity or pressure safety. The model listing is a source for this product’s stated purpose and range; the engineering decision belongs to the applicable inspection procedure.

Keep a record someone else can use

For a grid, number points clockwise from a fixed corner and keep a small sketch in the same folder as the readings. Mark ‘no stable echo’ rather than filling the cell with a guess. Repeat the lowest point after cleaning and couplant renewal. A map that preserves uncertainty is more useful to the engineer who decides what to inspect next.

A practical handover

Write down the exact model, the setup, the observation and the limit that still needs checking. For current version and buying information, use the Wintact WT100A product page.